Research/Patents/US 5118581
US 5118581

PROTECTION OF GAMMA TITANIUM ALUMINIDES WITH ALUMINOSILICATE COATINGS

Assignee

ROCKWELL INTERNATIONAL CORP.

Filed

Jul 26, 1990

Granted

Jun 2, 1992

Location

El Segundo CA (Aerospace Corp/TRW)

Abstract

A method and composition for protecting a gamma titanium aluminide alloy specimen subject to high temperature oxidation is disclosed. An alumino silicate glass coating is applied on the surface of the gamma titanium aluminide specimen. The coated specimen is heated to a temperature in a range of 2150°-2250° F. for a sufficient time period to form a silicide interfacial layer between the alloy and the glass coating. The glass coating is preferably a composition including SiO2 in a weight percentage of 60 to 65 Al2 O3 in a weight percent of 16 to 20. The glass coating results in minimal oxidation.

Source: Google Patents

35 USC §181 Secrecy Order

Imposed

Aug 22, 1991

Rescinded

Feb 4, 1992

Duration

5 months

Inventor

  • 1HODA SHALABY

Sensitive facility: El Segundo CA (Aerospace Corp/TRW)